Grade : IC1008

Used for High temp. alloys, stainless steel and hardened steel. Low to medium speed, iterrupted cut.

PropertyValue
ISO Range - P/M/K(P20-P50)(M20-M40)(K15-K40)
ISO Range - N/S/H (H20-H30)(S15-S25)(N05-N25)

PropertyValue
Grade or Coating TypePVD
Coating Layers TiAlN+TiN


Find group of specific workpiece material (opens in a new window)


Cutting Speed for: CCGT 09T3005-F1M-20P IC1008 - 3413508
ISOMaterialMaterial DesignationMaterial ConditionHardnessCutting Speed Recommendations (Vc)
P1Non-alloy steel and cast steel, free cutting steel <0.25%C.Annealed125 HB125-190 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%C.Annealed190 HB115-160 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55% CQuenched and tempered250 HB90-135 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55% CAnnealed220 HB100-155 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55% CQuenched and tempered.300 HB80-125 m/min
P6Low alloy and cast steel (less than 5% of alloying elements)Annealed200 HB100-155 m/min
P7Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered275 HB80-135 m/min
P8Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered300 HB80-125 m/min
P9Low alloy and cast steel (less than 5% of alloying elements)Quenched and tempered350 HB70-115 m/min
P10High alloyed steel, cast steel and tool steelAnnealed200 HB115-160 m/min
P11High alloyed steel, cast steel and tool steelQuenched and tempered325 HB70-115 m/min
P12Stainless steel and cast steelFerritic/martensitic200 HB100-180 m/min
P13Stainless steel and cast steelMartensitic240 HB100-190 m/min
M14Stainless steel and cast steelAustenitic, duplex180 HB80-155 m/min
K15Grey cast iron (GG)Pearlitic/ferritic180 HB80-150 m/min
K16Grey cast iron (GG)Pearlitic/martensitic260 HB70-105 m/min
K17Nodular cast iron (GGG)Ferritic160 HB75-125 m/min
K18Nodular cast iron (GGG)Pearlitic250 HB60-100 m/min
K19Malleable cast ironFerritic130 HB95-155 m/min
K20Malleable cast ironPearlitic230 HB75-125 m/min
S31High temp. alloys Fe basedAnnealed200 HB35-60 m/min
S32High temp. alloys Fe basedHardened280 HB25-40 m/min
S33High temp. alloys Ni or Co basedAnnealed250 HB25-40 m/min
S34High temp. alloys. Ni or Co basedHardened350 HB20-35 m/min
S35High temp. alloys. Ni or Co basedCast320 HB20-25 m/min
S36Titanium (pure)Pure190 HB90-155 m/min
S37Titanium alloysAlpha+beta alloys, hardened310 HB35-45 m/min
H38Hardened steelHardened55 HRC25-35 m/min
H39Hardened steelHardened60 HRC20-30 m/min
H40Chilled cast ironCast400 HB30-45 m/min
H41Cast ironHardened55 HRC30-40 m/min

Site Map

Groove-Turn & Parting  ISO-Turning   Threading   Milling   Hole Making   Reaming   Boring   Tooling Systems   Modular Adaptations  Multifunction Tools 

Terms of Use and Legal Disclaimer   Privacy Statement
© 2024 ISCAR LTD. Manufacturer of Metalworking Tools (Iscar.com) All Rights Reserved