GRADES AND MATERIALS
                                                     Material Groups

            According to DIN / ISO 513 and VDI 3323
                                                                                                            Material
                                                                 Tensile Strength                  Hardness   Group
              ISO          Material                Condition        [N/mm ]   Kc1  [N/mm ]  mc (2)   HB      No.
                                                                         2
                                                                                 (1)
                                                                                       2
                                    <0.25% C       annealed          420         1350       0.21     125      1
                                    ≥0.25% C       annealed          650         1525       0.22     190      2
               non-alloy steel and cast
               steel, free cutting steel  <0.55% C  quenched and tempered  850   1675       0.24     250      3
                                                   annealed
                                                                     750
                                                                                                              4
                                                                                 1675
                                                                                                     220
                                                                                            0.24
                                    ≥0.55% C
                                              quenched and tempered  1000        1900       0.24     300      5
                                                   annealed          600         1775       0.24     200      6
             P low alloy and cast steel                              930         1675       0.24     275      7
               (less than 5% of alloying elements)  quenched and tempered  1000  1725       0.24     300      8
                                                                     1200        1800       0.24     350      9
                                                   annealed          680         2450       0.23     200      10
               high alloyed steel, cast steel and tool steel
                                              quenched and tempered  1100        2500       0.23     325      11
                                                ferritic / martensitic  680      1875       0.21     200      12
               stainless steel and cast steel
                                                   martensitic       820         1875       0.21     240      13
             M stainless steel and cast steel    austenitic, duplex  600         2150       0.20     180      14
                                                 ferritic / pearlitic            1150       0.20     180      15
               gray cast iron (GG)
                                                pearlitic / martensitic          1350       0.28     260      16
                                                    ferritic                     1225       0.25     160      17
             K nodular cast iron (GGG)
                                                    pearlitic                    1350       0.28     250      18
                                                    ferritic                     1225       0.25     130      19
               malleable cast iron
                                                    pearlitic                    1420       0.3      230      20
                                                 not hardenable                   700       0.25     60       21
               aluminum-wrought alloys
                                                   hardenable                     800       0.25     100      22
                                                 not hardenable                   700       0.25     75       23
                                    ≤12% Si
               aluminum-cast alloys                hardenable                     700       0.28     90       24
                                    >12% Si      high temperature                 750       0.25     130      25
             N
                                    >1% Pb         free cutting                   700       0.27     110      26
               copper alloys                         brass                        700       0.27     90       27
                                                electrolytic copper               700       0.27     100      28
                                              duroplastics, fiber plastics        200       0.20   70 Shore D  29
               non metallic
                                                   hard rubber                    200       0.20   55 Shore D  30
                                                   annealed                      2600       0.24     200      31
                                    Fe based
                                                   hardened                      3100       0.24     280      32
               high temperature alloys             annealed                      3300       0.24     250      33
             S                      Ni or Co       hardened                      3300       0.24     350      34
                                    based
                                                     cast                        3300       0.24     320      35
                                                     pure            400         1160       0.24     190      36
               titanium alloys
                                             alpha+beta alloys, hardened  1050   1245       0.24     310      37
                                                   hardened                      4600       0.25    55 HRC    38
               hardened steel
             H                                     hardened                      4700       0.25    60 HRC    39
               chilled cast iron                     cast                        4600       0.27     400      40
               cast iron                           hardened                      4500       0.27    55 HRC    41
                steel
                stainless steel
                cast iron
                non-ferrous metals
                superalloys and titanium
                hard materials
            (1)  Specific cutting force for 1 mm 2  chip section.