USER GUIDE


             Machining Data for Threading
                                                                                              Coated
                                                        Tensile          Material    IC228  IC908  IC808    IC1007       THREADING
                                                       Strength  Hardness   Group
               ISO      Material           Condition     [ksi]    HB      No.            Cutting Speed (SFM)
                              <0.25% C      Annealed     61      125      1     200 - 330  380 - 620  410 - 670  440 - 750
                              ≥0.25% C      Annealed     94      190      2     200 - 310  360 - 590  390 - 640  430 - 720
                Non-alloy steel   <0.55% C  Quenched and   123   250      3     160 - 300  330 - 570  340 - 610  390 - 690
                and cast steel,             tempered
                free cutting steel          Annealed     109     220      4     150 - 280  300 - 540  310 - 570  360 - 660
                              ≥0.55% C    Quenched and
                                            tempered     145     300      5     150 - 280  300 - 540  310 - 570  360 - 660
                                            Annealed     87      200      6     160 - 310  330 - 590  340 - 640  390 - 710
              P
                Low alloy and cast steel (less           135     275      7     130 - 250  250 - 460  260 - 490  300 - 560
                than 5% of alloying elements)  Quenched and   145  300    8     110 - 230  230 - 440  250 - 480  280 - 520
                                            tempered
                                                         174     350      9     110 - 230  230 - 440  250 - 480  280 - 520
                                            Annealed     99      200      10    130 - 210  260 - 390  280 - 430  310 - 480
                High alloyed steel, cast
                steel and tool steel      Quenched and   160     325      11    80 - 160  160 - 330  180 - 340  200 - 390
                                            tempered
                                         Ferritic/martensitic  99  200    12    110 - 230  230 - 430  250 - 460  280 - 510
                Stainless steel and cast steel
                                           Martensitic   119     240      13    150 - 200  280 - 360  300 - 390  330 - 430
             M Stainless steel and cast steel  Austenitic, duplex  87  180  14  150 - 250  300 - 460  310 - 490  360 - 560
                                         Ferritic / pearlitic    180      15    210 - 280  410 - 520  440 - 560  490 - 620
                Gray cast iron (GG)
                                        Pearlitic / martensitic  260      16    150 - 210  300 - 390  310 - 430  360 - 480
                                             Ferritic            160      17    110 - 230  230 - 430  250 - 460  280 - 510
             K Nodular cast iron (GGG)
                                            Pearlitic            250      18    100 - 200  200 - 380  210 - 410  230 - 460
                                             Ferritic            130      19    100 - 110  200 - 230  210 - 250  230 - 280
                Malleable cast iron
                                            Pearlitic            230      20    100 - 250  200 - 480  210 - 510  230 - 570
                                          Not hardenable          60      21    160 - 640  330 - 1200 340 - 1280 390 - 1440
                Aluminum-wrought alloys
                                           Hardenable            100      22    130 - 380  260 - 720  280 - 770  310 - 870
                                          Not hardenable          75      23    340 - 710  660 - 1310 710 - 1410 790 - 1570
                Aluminum-     ≤12% Si      Hardenable             90      24    340 - 490  660 - 920  710 - 980  790 - 1100
                cast alloys
                              >12% Si    High temperature        130      25    340 - 490  660 - 920  710 - 980  790 - 1100
             N                >1% Pb       Free cutting          110      26    130 - 440  260 - 840  280 - 900  310 - 1000
                Copper alloys                Brass                90      27    130 - 440  260 - 840  280 - 900  310 - 1000
                                         Electrolytic copper     100      28    130 - 440  260 - 840  280 - 900  310 - 1000
                                          Duroplastics,                   29    130 - 430  260 - 820  280 - 870  310 - 980
                Non metallic               fiber plastics
                                           Hard rubber                    30    130 - 430  260 - 820  280 - 870  310 - 980
                                            Annealed             200      31    80 - 100  150 - 200  160 - 210  180 - 230
                              Fe based
                                           Hardened              280      32     50 - 80  110 - 160  110 - 180  130 - 200
                High temperature            Annealed             250      33     30 - 50  70 - 100  70 - 100  80 - 110
                alloys        Ni or Co     Hardened              350      34     20 - 30  50 - 80  50 - 80  60 - 100
              S               based
                                             Cast                320      35     20 - 30  50 - 80  50 - 80  60 - 100
                                             Pure        58      190      36    250 - 300  460 - 560  490 - 590  560 - 670
                Titanium alloys          Alpha+Beta alloys,   152  310    37    80 - 110  160 - 230  180 - 250  200 - 280
                                            hardened
                                           Hardened             55 HRC    38    80 - 100  150 - 200  160 - 210  180 - 230
                Hardened steel
             H                             Hardened             60 HRC    39    80 - 100  150 - 200  160 - 210  180 - 230
                Chilled cast iron            Cast                400      40    80 - 100  150 - 200  160 - 210  180 - 230
                Cast iron                  Hardened             55 HRC    41    80 - 100  150 - 200  160 - 210  180 - 230