Page 55 - MILLING_CATALOG_INCH_2022_P361-P592
P. 55
USER GUIDE
Machining Data for Slitting with SELF-GRIP and TANGSLIT Cutters
Coated Uncoated
Tensile Material IC928/ IC908/
Strength Hardness Group IC328 IC830 IC808 IC20 (SFM)
ISO Material Condition [ksi] HB No. (1) (SFM) (SFM) (SFM)
<0.25% C Annealed 61 125 1 A 560-660 A 750 max B 640-820
≥0.25% C Annealed 94 190 2 A 390-560 A 660 max B 460-750
Non-alloy steel <0.55% C Quenched and 123 250 3 A 390-560 B 460-750
and cast steel, tempered A 520 max
free cutting steel Annealed 109 220 4 A 300-460 A 520 max B 340-610
≥0.55% C Quenched and 145 300 5 A 300-490 B 340-640 SLOTTING & SLITTING CUTTERS
tempered A 520 max
Annealed 87 200 6 A 390-520 A 590 max B 460-690
P Low alloy and cast steel 135 275 7 A 330-460 B 380-610
(less than 5% of Quenched and A 520 max
alloying elements) tempered 145 300 8 A 260-460 A 520 max B 300-610
174 350 9 A 230-330 A 360 max B 260-390
Annealed 99 200 10 A 200-260 A 300 max B 250-380
High alloyed steel, cast
steel and tool steel Quenched and 160 325 11 A 180-230 A 260 max B 150-330
tempered
Ferritic/martensitic 99 200 12 260-390 300-490 230-590
Stainless steel and cast steel
Martensitic 119 240 13 200-300 230-390 200-520
M Stainless steel and cast steel Austenitic, duplex 87 180 14 200-300 230-390 200-520
Ferritic / pearlitic 180 15 300-460 230-360
Gray cast iron (GG) Pearlitic / 260 16 230-330 180-260
martensitic
K Ferritic 160 17 380-460 310-360
Nodular cast iron (GGG)
Pearlitic 250 18 300-390 230-330
Ferritic 130 19 380-460 310-360
Malleable cast iron
Pearlitic 230 20 300-390 230-330
Not hardenable 60 21 820
Aluminum-wrought alloys
Hardenable 100 22 820
Not hardenable 75 23 820
Aluminum- ≤12% Si
cast alloys Hardenable 90 24 820
>12% Si High temperature 130 25 820
N >1% Pb Free cutting 110 26 820
Copper alloys Brass 90 27 820
Electrolytic copper 100 28 820
Duroplastics,
Non metallic fiber plastics 29
Hard rubber 30
Annealed 200 31 130-160 100-130
Fe based
High temperature Hardened 280 32 100-130 70-100
alloys Ni or Co Annealed 250 33 100-130 70-100
S based Hardened 350 34 100-130 70-100
Cast 320 35 70-100 50-80
Pure 58 190 36 100-130 50-80
Titanium alloys Alpha+Beta
alloys, hardened 152 310 37 100-130 70-100
Hardened 55 HRC 38 80-160
Hardened steel
H Hardened 60 HRC 39 100-130
Chilled cast iron Cast 400 40 160-200 30-70
Cast iron Hardened 55 HRC 41 100-160
For machining aluminum, use IC20, maximum cutting speed corresponds to the maximum RPM indicated on the cutter A - First choice B - Second choice
Recommendations are for normal machining conditions
If excessive wear occurs, select insert with higher hardness
If chipping or breakage occurs, select insert with more toughness
(1) For workpiece materials list, see pages 806-837
415