Page 40 - Solid_Brochure_2021_INCH
P. 40
Slotting
Slotting
Cutting Diameter Feed (IPT) Axial
Material No. Cutting Speed Recommendations Hardness HB
ISO Material Condition (Vc) SFM 1/8 3/16 1/4 5/16 3/8 7/16 1/2 5/8 3/4 1 ap max
1 Non-alloy Annealed 890-960 125 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
2 steel and <.25%C Annealed 710-815 190 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
3 cast steel, Quench and tempered 570-780 250 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
4 free cutting >=.55%C Annealed 570-780 220 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
Dimensions
5 steel >=.55%C Quenched & tempered 500-635 300 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
6 Annealed 570-780 200 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD IC608
Low alloy & cast
OAL
RE
DCONMS
NOF
DC
Designation Quenched & tempered 425-635 LU 275 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
Shank
APMX
(1)
7
P
steel (less than 5% of
8
4.1250 300 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024
1.000
4.1250
ECI-5 1.-4.13W0VF7 Quenched & tempered 450-635 0 1.000 7.000 5 W 1xD •
alloying elements)
1.0000 350 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024
9
ECI-5 .25-1.C.06VF3 Quenched & tempered 500-635 .0600 999.000 3.000 5 C 1xD •
1.0000
.250
10 High alloyed steel,
(1) Number of flutes Annealed 450-635 200 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
11
cast steel and tool steel
• Weldon shank available upon request. Substitute a W in place of the C in the listed designations (example - ECI-4 375-1.0C03VF2.5 = cylindrical type; ECI-4 .0024 1xD
240-425 325 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018
Quenched & tempered
12 Stainless steel
375-1.0W03VF2.5 = Weldon type Ferritic/martensitic 280-570 200 .0003 .0004 .0006 .0007 .0009 .0020 .0012 .0015 .0018 .0024 1xD
13 and cast steel Martensitic 210-530 240 .0003 .0004 .0006 .0007 .0009 .0020 .0012 .0015 .0018 .0024 1xD
Stainless steel
M 14 and cast steel Austenitic 210-425 180 .0003 .0004 .0006 .0007 .0009 .0020 .0012 .0015 .0018 .0024 1xD
15 Grey cast iron (GG) Pearlitic/ferritic 280-890 180 .0003 .0004 .0006 .0007 .0009 .0030 .0012 .0015 .0018 .0024 1xD
16 Pearlitic/martensitic 450-850 260 .0003 .0004 .0006 .0007 .0009 .0030 .0012 .0015 .0018 .0024 1xD
17 Ferritic 530-960 160 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
K 18 Nodular cast iron (GGG) Pearlitic 530-960 250 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
19 Malleable cast iron Ferritic 530-960 130 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
20 Pearlitic 500-850 230 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
31 Fe based Annealed 70-145 200 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
32 High temp. Cured 70-110 280 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
33 alloys Ni or Co Annealed 70-110 250 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
S 34 based Cured 70-110 350 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
35 Cast 70-110 320 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
36 Titanium Ti alloys Pure 110-280 310 .0003 .0004 .0006 .0007 .0009 .0020 .0012 .0015 .0018 .0024 1xD
37 Alpha+beta alloys cured 80-280 310 .0003 .0004 .0006 .0007 .0009 .0010 .0012 .0015 .0018 .0024 1xD
Roughing Cutting Diameter Feed (IPT) Profiling Radial
Material No. Cutting Speed Recommendations (Vc) SFM Hardness HB
ISO Material Condition 1/8 3/16 1/4 5/16 3/8 7/16 1/2 5/8 3/4 1 ap ae
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
1 <.25%C Annealed 890-960 125 .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
2 Non-alloy >=.25%C Annealed 710-815 190 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
steel and
3 cast steel, <.55%C Quench and 570-780 250 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
.0006 .0008
.001
tempered
.0004
.0024 .0031
1.5xD
.0012 .0014 .0016
.002
free cutting
4 steel >=.55%C Annealed 570-780 220 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Quenched .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
5 >=.55%C 500-635 300 .25xD-.4xD
& tempered .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
6 Annealed 570-780 200 .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Quenched .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
P 7 Low alloy & cast & tempered 425-635 275 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
steel (less than 5%
8 of alloying elements) Quenched 450-635 300 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
& tempered .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Quenched .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
9 500-635 350 .25xD-.4xD
& tempered .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
10 High alloyed Annealed 450-635 200 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
steel, cast steel
11 and tool steel Quenched 240-425 325 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
& tempered .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Ferritic/ 280-570 200 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
12
40 ISCAR FLASHLINE High Productivity Tools Combined With a Great Economical Advantage
.002
.0006 .0008
.001
.0024 .0031
1.5xD
Stainless steel
.0004
.0012 .0014 .0016
martensitic
13 and cast steel Martensitic 210-530 240 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Stainless steel .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
M 14 Austenitic 210-425 180 .25xD-.4xD
and cast steel .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Pearlitic/ .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
15 ferritic 280-890 180 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
Grey cast iron (GG)
16 Pearlitic/ 450-850 260 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
martensitic .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
17 Ferritic 530-960 160 .25xD-.4xD
.0004
.002
.001
.0006 .0008
.0012 .0014 .0016
1.5xD
.0024 .0031
K Nodular cast .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
18 iron (GGG) Pearlitic 530-960 250 .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
19 Ferritic 530-960 130 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
Malleable cast iron
20 Pearlitic 500-850 230 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
31 Annealed 70-145 200 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
Fe based
32 Cured 70-110 280 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
High temp. .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
33 Annealed 70-110 250 .25xD-.4xD
alloys .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Ni or Co .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
S 34 based Cured 70-110 350 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
35 Cast 70-110 320 .25xD-.4xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
.00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
36 Pure 110-280 310 .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .25xD-.4xD
Titanium Ti alloys Alpha+beta .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
37 80-280 310 .25xD-.4xD
alloys cured .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
55 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
38 Hardened 110-210 HRC .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD .02xD
Hardened Steel
39 Hardened 110-145 60 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .02xD
H HRC .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
40 Chilled Cast Iron Cast 250-320 400 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD- .02xD
.0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
55 .00035- .0005- .0007- .0008- .001- .0011- .0013- .0016- .0019- .0026- .75xD-
41 Cast Iron Hardened 110-210 .02xD
HRC .0004 .0006 .0008 .001 .0012 .0014 .0016 .002 .0024 .0031 1.5xD
Semi-Finish Profiling
Material No. Cutting Speed Recommendations (Vc) SFM Hardness HB Cutting Diameter Feed (IPT) Radial
ISO Material Condition 1/8 3/16 1/4 5/16 3/8 7/16 1/2 5/8 3/4 1 ap ae
1 >=.25%C Annealed 890-960 125 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
2 Annealed 710-815 190 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
Non-alloy Quench and
3 <.55%C 570-780 250 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
steel and cast tempered
4 steel, free >=.55%C Annealed 570-780 220 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
cutting steel Quenched &
5 500-635 300 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
>=.55%C tempered
6 Annealed 570-780 200 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
Quenched &
P 7 tempered 425-635 275 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
Low alloy & cast
8 steel (less than 5% of Quenched & 450-635 300 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
tempered
alloying elements) Quenched &
9 500-635 350 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
tempered
10 Annealed 450-635 200 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
High alloyed steel,
11 cast steel and tool steel Quenched & 240-425 325 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
tempered
12 Stainless steel Ferritic/martensitic 280-570 200 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
13 and cast steel Martensitic 210-530 240 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
Stainless steel
M 14 Austenitic 210-425 180 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
and cast steel
15 Grey cast iron (GG) Pearlitic/ferritic 280-890 180 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
16 Pearlitic/martensitic 450-850 260 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
17 Ferritic 530-960 160 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
K Nodular cast iron (GGG)
18 Pearlitic 530-960 250 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
19 Malleable cast iron Ferritic 530-960 130 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
20 Pearlitic 500-850 230 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
31 Fe based Annealed 70-145 200 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
32 High temp. Cured 70-110 280 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
33 alloys Ni or Co Annealed 70-110 250 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
S 34 based Cured 70-110 350 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
35 Cast 70-110 320 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
36 Pure 110-280 310 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
Titanium Ti alloys Alpha+beta
37 80-280 310 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .05xD
alloys cured
38 Hardened Steel Hardened 110-210 55 HRC .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .02xD
H 39 Hardened 110-145 60 HRC .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .02xD
40 Chilled Cast Iron Cast 250-320 400 .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .02xD
41 Cast Iron Hardened 110-210 55 HRC .0009 .0013 .0017 .0021 .0025 .0030 .0034 .0042 .0050 .0068 1xD .02xD